FIXMASTER FLEX 80
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- Two-Part Black Urethane
- Casting and Rebuilding Parts
- Corrosion, Wear, and Impact Exposure
Product Description
LOCTITE MR FLEX 80 is a two-part, thick black polyurethane compound for casting and rebuilding parts exposed to corrosion, wear, and impact. LOCTITE MR FLEX 80 is the current designation associated with the former FIXMASTER FLEX80 name. It is used for repair by casting and rebuilding parts subject to corrosion, wear, or impact exposure. Its product role is repair and casting rather than general-purpose structural bonding.
Key features
- Two-Part Black Urethane: The material is a thick black polyurethane compound supplied as a two-part system.
- Casting and Rebuilding Parts: The castable system is used to rebuild and repair parts.
- Corrosion, Wear, and Impact Exposure: The castable urethane is used on parts exposed to corrosion, wear, and impact.
Applications
Casting and rebuilding parts exposed to corrosion, wear, and impact.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
AppearanceAppearance
Thick black liquidComponent SystemComponent System
Two Part (Resin | Hardener)Mechanical Properties
ElongationElongation
237 %Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
<-50 °CThermal ConductivityThermal Conductivity
0.16 W/m.KElectrical Properties
Volume ResistivityVolume Resistivity
15×10¹² Ohms⋅cmOther Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C