FREKOTE C-210

Harmonization Code : 3215907090 | Ink, whether or not concentrated or solid (excl. printing ink, printer/copier ink cartridges incorporating mechanical or electrical components, and solid ink in engineered shapes for printers/copiers)

FREKOTE C-210

Main features

  • Above 60 deg C Hot-Mold Touch-Up
  • Ready-to-Use No-Mix Emulsion
  • Spray, Brush, Wipe, or Dip

Product Description

LOCTITE FREKOTE C-210 is a water-based mold release product for hot-mold touch-up and spray application over a LOCTITE FREKOTE C-200 base coat. It is intended for touch-up on molds above 60 deg C or where spray application is used. The product is supplied ready to use, requires no mixing, and provides multiple releases without contaminating transfer to molded parts. It is a white emulsion with typical specific gravity of 1.00; application methods include spray, brush, wipe, or dip.

Key features

  • Hot-Mold Touch-Up: The product is intended for touch-up on molds above 60 deg C.
  • Ready-to-Use No-Mix Emulsion: The product is a white water-based emulsion with typical specific gravity of 1.00 and requires no mixing.
  • Spray, Brush, Wipe, or Dip: Spray is recommended for hot-mold touch-up; brush, wipe, and dip are alternative application methods.

Applications

Hot-mold touch-up; spray-applied mold release; use over a LOCTITE FREKOTE C-200 base coat.

Product Family

FREKOTE C-210

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
White emulsion
Specific GravitySpecific Gravity
1.00
Other Properties
Storage TemperatureStorage Temperature
Below 40 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical C-210 as-supplied values from the manufacturer-authored C-200/C-210 product description sheet.

PropertyValueUnitMethod / condition
AppearanceWhite emulsion-As supplied
OdorSlight mild-As supplied
Specific gravity1.00-Typical C-210 value
Storage limitBelow 40deg CSpecial caution in exact product sheet

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers