- pH 5.6 Blue Liquid
- Complete Water Solubility
- 1.0 to 1.1 Specific Gravity
Product Description
INDICATOR 11 is a Henkel auxiliary liquid sold under IDH 592402. It is a blue, odorless liquid with pH 5.6, complete water solubility, and typical specific gravity from 1.0 to 1.1. Use of INDICATOR 11 in a specific process bath or titration requires an INDICATOR 11-specific procedure. Application instructions, bath concentrations, addition rates, and operating limits from other indicator products should not be applied to INDICATOR 11.
Key features
- Blue, Odorless Auxiliary Liquid: As supplied, INDICATOR 11 has pH 5.6.
- Complete Water Solubility: The auxiliary solution is completely soluble in water in its as-supplied state.
- Typical Specific Gravity: Typical specific gravity is 1.0 to 1.1.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
ColorColor
BlueSpecific GravitySpecific Gravity
1.0 - 1.1Thermal Properties
Boiling PointBoiling Point
> 98.9 °CFlash PointFlash Point
> 98.9 °C