HumiSeal 1B18 Acrylic Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal 1B18 Acrylic Conformal Coating

Main features

  • Single‑component acrylic formulation
  • Excellent flexibility
  • RoHS compliant & UL recognized

Product Description

HumiSeal 1B18 is a single‑component, fast‑drying acrylic conformal coating formulated for use on printed circuit assemblies. It provides excellent flexibility and electrical insulation performance, fluoresces under UV light for simplified inspection, and is easily repairable. HumiSeal 1B18 is compliant with RoHS Directive 2002/95/EC and is recognized under UL File Number E105698.

Product Key Features

  • Single‑component acrylic formulation
  • Fast drying for efficient processing
  • Excellent flexibility to withstand thermal and mechanical stress
  • RoHS compliant (Directive 2002/95/EC)
  • UL recognized (File No. E105698)

Applications

  • Protection of printed circuit boards (PCBs) in consumer, industrial, and automotive electronics
  • Use in high‑reliability electronics requiring quick processing and strong dielectric performance
Product Family

HUMISEAL 1B18

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)Density (g)
0.92 g/cm3
Film ThicknessFilm Thickness
25 - 75 µm
SolidsSolids
30 %
Physical Properties
ViscosityViscosity
250 mPa.s
Thermal Properties
Operating TemperatureOperating Temperature
-65 - 125 °C
UL 94 RatingUL 94 Rating
V-0
Electrical Properties
Breakdown VoltageBreakdown Voltage
6300 V

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers