Hysol GR510 | Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other


Main features
- High filler loading
- Ultra low CTE of 8 ppm/°C
- Designed for Quad Flat Pack (QFP) devices
Product Description
Hysol GR510 is a black, ultra-low CTE, transfer molded semiconductor epoxy molding compound designed for thin and larger quad flat pack (QFP) and larger small outline transistor (SOT) packages . Once transfer molded and post-mold cured, it has a very low CTE, low moisture absorption and high adhesion to a range of leadframe types. This allows it to acheive very high reliability levels for quad flat pack devices, but also for a range of larger SOIC packages.
Hysol GR510 has an ultra low coefficient of thermal expansion (CTE) of 8 ppm/°C that makes it one of the lowest stress materials avaiable in an epoxy molding compound. This low CTE comes from a technical breakthrough in filler size, filler type and filler loading. It has been successfully used for the production of printer heads from industry leading companies.
Hysol GR510 is an environmentally "green" product, meaning that it doesn't contain any bromine, antimony or phosphorus flame retardants. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on quad flat pack devices and other, larger small outline packages including SOT, SOD and SMX package types. Hysol GR510 meets UL 94 V-0 Flammability at 1/8 inch (3.175mm) thickness.
Packaging
Technical Specifications
General Properties
Electrical Properties
Thermal Properties
Chemical Properties
Curing Conditions
Physical Properties
Additional Information
GR510 is a product that can replace GR828-FC1 for power SOTs. FC initials might remind you of Fairchild. Fairchild has been acquired by Onsemi in 2017 so their products still live on.