Hysol GR600 SL2| Black Epoxy Mold Compound
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Main features
- High reliability
- High power applications
- Good electrical performance
Product Description
Hysol GR600 SL2 is a halogen free, black, silica filled (87% filler weight) semiconductor grade epoxy molding compound designed for TO packages. This low stress, low moisture absorption product is a commercial success with many uses on TO applications.
Hysol GR600 SL2 is a green, heat curable epoxy molding compound that can be used in semiconductor packages such as TO252. Furthermore, it meets UL 94 V-0 flammability at 1/8 inch thickness.
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
ColorColor
BlackFiller ContentFiller Content
87 %Specific GravitySpecific Gravity
2.03Electrical Properties
Volume ResistivityVolume Resistivity
14400000000000000 Ohms⋅cmChemical Properties
Moisture absorptionMoisture absorption
0.30 %Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
83 cmThermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
165 °CCuring Conditions
Transfer PressureTransfer Pressure
40 - 85 kg/cm2Transfer TimeTransfer Time
5 - 15 s