Hysol GR640HV-L1 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR640HV-L1 Black Epoxy Mold CompoundHysol GR640HV-L1 | Black Epoxy Mold CompoundGR640HV-L1 Black Epoxy Mold Compound

Main features

  • Improved electrical performance version of GR640HV
  • Ideal for TO, SMX and SOT/SOD Packages
  • JEDEC 1 260°C capable product

Product Description

Hysol GR640HV-L1 is a black, heat-curable epoxy molding compound that delivers outstanding performance and ease of use. This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature.  It is an improved version of GR640HV with better electrical performance version. 

Hysol GR 640HV-L1 is a "Green" low stress product with low cost of ownership that meets the strict MSL1 JEDEC requirements. It is designed for  semiconductor discrete packages such as TO220, TO247 and other TO packages, SMA, SMB and other SMX packages and Transformers. It is developed for eutectic bonding and not for die attach bonding. In eutectic bonding, an intermediate metal layer that forms a eutectic composition with either or both of the bonded components is used. Eutectic bonding is a low-temperature process, which is beneficial for temperature-sensitive applications where high temperatures affect the integrity of the device components. It is important to check the compatibility of Hysol GR640HV-L1 with the bonding process to maximize its excellent moisture sensitivity capability. GR640HV-L1 meets UL 94 V-0 Flammability at ¼ inch thickness.

 
Product Family

HYSOL GR640HV-L1

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Black
Filler ContentFiller Content
78 %
Specific GravitySpecific Gravity
1.88
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
178 °C
UL 94 RatingUL 94 Rating
V0
Electrical Properties
Volume ResistivityVolume Resistivity
12000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
0.4 %
Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
140 cm

Additional Information

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers