Hysol MG33F-0520 | Gold Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

MG33F-0520 Gold Epoxy Mold CompoundHysol MG33F-0520 | Gold Epoxy Mold Compound

Main features

  • Lasemark capability
  • Low moisture absorption
  • Solvent resistant

Product Description

Hysol MG33F-0520 is a first generation gold epoxy molding compound that is specifically designed for use in high volume molding of tantalum capacitors. It is a silica filled, environmentally friendly 'green' molding compound with high thermal cycling stability, low stain and low moisture absorption. It has been successfully used for surface mount Mno2 tantalum capacitors and reed relays. Its solvent resistance makes it suitable for use with automotive fluids such as mineral spirits and ethylene glycol.

Hysol MG33F-0520 has excellent moldability and fast cycle times while also offering lasermark capabilities. It has low levels of ionic contaminants, excellent adhesion to copper and is stable after multiple thermal cycles. The main difference from MG33 is that it contains a flame retardant (F) which allows it to meet the UL94 V-0 flammability rating.

 

Curing Time

  • 30 to 45 seconds @170°C
  • 1.0 to 1.5 minutes @150°C

Post Cure

  • 2 hours @150°C
Product Family

HYSOL MG33F-0520

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Gold
Specific GravitySpecific Gravity
1.87
Electrical Properties
Volume ResistivityVolume Resistivity
12500000000000000 Ohms⋅cm
Chemical Properties
Water Extract ConductivityWater Extract Conductivity
0.000021 Ohm
Water Extract pHWater Extract pH
6.5
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
170 °C
UL 94 RatingUL 94 Rating
V0
Curing Conditions
Transfer PressureTransfer Pressure
35 - 105 kg/cm2

Additional Information

This product claims low moisture absorption. Can it withstand X parameters for Y years?

MG33F-0520 water absorption test is 0.6% by weight (Pressure Cooker Test for 24 hours @ 121°C). This data cannot be translated into product lifetime as there are still many variables to determine the life of the device (experimental and computational modeling).  What we actually need is a test during qual on HAST and/or Autoclave. Customers have different ways of extrapolating and predicting the lifetime of the device.

There are many moisture-related failure modes and several tests can be conducted to determine the likelihood of a failure mode occurring. Ultimately, Molding compounds, any of them, are semi-permeable materials that are always susceptible to moisture. It will highly depend on storage conditions, handling, equipment packaging etc. 

Filler loading and resin type, can also help understand the molding compound's ability to absorb or resist moisture. A filer with more than 70% is resistant to moisture. This is one approach to make the material moisture-resistant. MG33F-0520 has 74%. On the other hand the best resin to resist moisture is Biphenyl based. MG33F-0520 is not that. The resin system is EOCN (O-Cresol Novolac Epoxy Resin)+PN. 

Based on this information we assume an MSL3 level will be hard to attain. We recommend baking the molded device at 125C for 2 hours. This removes moisture and provides confidence to the package's lifetime. 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers