INSULCURE 20

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

I-CURE 20

Main features

  • Low-Viscosity Epoxy Hardening
  • 60-Minute Pot-Life Window
  • Rapid Ambient-Temperature Cure

Product Description

Insulcure 20 is a low-viscosity epoxy curing agent for use as a hardener in epoxy systems. The supplied material has a viscosity of 700 cP at 25 deg C by ASTM D2393 and a 60-minute pot life. The cure schedule is 16 hours at 25 deg C. The product combines good impact performance with rapid cure, providing a fluid curing-agent option where a one-hour processing window is useful. As a standalone curing-agent product, it is intended for epoxy curing applications.

Key features

  • Low supplied viscosity: Viscosity is 700 cP at 25 deg C by ASTM D2393.
  • One-hour pot life: Pot life is 60 minutes.
  • Rapid ambient cure: The cure schedule is 16 hours at 25 deg C.

Applications

Epoxy curing and hardening.

Product Family

INSULCURE 20

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Amber
Density (g)Density (g)
0.98 g/cm3
Vapor PressureVapor Pressure
<1 mmHg
Thermal Properties
Boiling PointBoiling Point
>190 °C
Flash PointFlash Point
>126.0 °C
Physical Properties
VOCVOC
0

Additional Information

Technical properties

As-supplied / before-processing properties

Values are product-selection data for the curing agent and are not specifications.

PropertyValueUnitMethod / condition
Viscosity700cP25 deg C; ASTM D2393
Pot life60minCondition not stated
Cure schedule16h25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers