INSULCURE 26

Main features

  • Very-Large-Casting Epoxy Hardening
  • Extended 120-Minute Pot-Life Window
  • Low-Viscosity Material Handling

Product Description

Insulcure 26 is an epoxy curing agent for very large castings and good impact performance. Supplied viscosity is 800 cP at 25 deg C by ASTM D2393, while the 120-minute pot life provides a longer working window for casting preparation. The cure schedule is 36 hours at 25 deg C. Supplied as a single hardener product, Insulcure 26 is used with epoxy systems where extended processing time is required for large casting operations.

Key features

  • Very large casting use: The curing agent is intended for very large castings.
  • Extended pot life: Pot life is 120 minutes.
  • Low supplied viscosity: Viscosity is 800 cP at 25 deg C by ASTM D2393.

Applications

Epoxy curing and hardening for very large castings.

Product Family

INSULCURE 26

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Amber
Specific GravitySpecific Gravity
0.94
Vapor PressureVapor Pressure
<1 mmHg
Thermal Properties
Boiling PointBoiling Point
> 160 °C
Flash PointFlash Point
232.2 °C
Physical Properties
VOCVOC
0

Additional Information

Technical properties

As-supplied / before-processing properties

Values are product-selection data for the curing agent and are not specifications.

PropertyValueUnitMethod / condition
Viscosity800cP25 deg C; ASTM D2393
Pot life120minCondition not stated
Cure schedule36h25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers