FM-7711 | Reactive PDMS - Bi terminal Methacryloxy

Harmonization Code : 3910.00.00.60 | Polydimethylsiloxane, whether or not polyethylene glycol and trifluoropropyl substituted, with methacrylate end groups

FM-7711 | Reactive PDMS - Bi terminal Methacryloxy

Main features

  • Bi terminal
  • 1,000 g/mol | 18 mPas
  • Methacryloxy functional groups

Product Description

Silaplane® FM-7711 is a reactive polydimethylsiloxane (PDMS) based polymer with a molecular weight of 1,000 g/mol and a Viscosity of 18 mPas. This reactive silicone material offers the addition of silicone-type properties to non-Silicone materials in a variety of industries including electronics, semiconductors, automotive, biotech, healthcare, and clean energy applications. It offers narrow polydispersity and a low level of chemical impurities.

Silaplane® FM-7711 bi-terminal product has two Methacryloxy functional groups that are reactive toward a variety of compounds and surfaces enabling chemical and physical changes to chemicals, particle surfaces and larger surface structures. Methacryloxy groups are mainly compatible with Acrylic resins.

Product Family

JNC FM-7711

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Molecular weightMolecular weight
1000 g/mol
Specific GravitySpecific Gravity
0.98
Physical Properties
ViscosityViscosity
18 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers