KANEKA GR6824

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

KANEKA GR6824

Main features

  • Room-Temperature Filament Winding
  • High-Strain Composite Capability
  • Six-Hour 140 deg F Cure

Product Description

Kaneka GR6824 is an epoxy composite resin grade for filament winding, including room-temperature winding operations. Initial viscosity is 680 cP at 77 deg F, and the cure schedule is 6 hours at 140 deg F. The cured material reaches a glass transition temperature of 163 deg F (73 deg C) and has high strain capability. This product is the epoxy resin grade only; a curing agent is not included. Its room-temperature winding use, defined cure schedule, and strain capability provide a focused processing profile for filament-wound composite parts.

Key features

  • Room-temperature winding: The grade is used for filament winding at room temperature.
  • High strain capability: The cured composite system is characterized by high strain capability.
  • Defined cure schedule: The cure schedule is 6 hours at 140 deg F.

Applications

Filament winding and room-temperature winding of composite parts.

Product Family

KANEKA GR6824

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
ViscosityViscosity
680 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
73 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are product-selection data for the resin grade and are not specifications.

PropertyValueUnitMethod / condition
Resin typeEpoxyAs supplied
Initial viscosity680cP77 deg F
Cure schedule6h140 deg F

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers