Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

KANEKA GR6840

Main features

  • Toughened Wet-Lamination Processing
  • High Delamination Resistance
  • Thin-to-Thick Composite Part Production

Product Description

Kaneka GR6840 is a toughened epoxy composite resin grade for wet lamination. Initial viscosity is 1,200 mPa*s at 77 deg F, and working life is 50 minutes before viscosity doubles. The cure temperature is 176 deg F (80 deg C). Cured-system data include an 81 deg C glass transition temperature, 123 MPa flexural strength, and 2.9 GPa flexural modulus. The grade resists delamination and can be used for thin or thick laminated parts. This product is the epoxy resin grade only; a curing agent is not included.

Key features

  • Toughened lamination resin: The epoxy grade is formulated for wet lamination.
  • Delamination resistance: The cured composite system provides resistance to delamination.
  • Thin-to-thick part use: The resin can be used for thin or thick laminated parts.

Applications

Wet lamination of thin and thick composite parts.

Product Family

KANEKA GR6840

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
ViscosityViscosity
1,200 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
82 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are product-selection data and are not specifications. Working life is the time for viscosity to double.

PropertyValueUnitMethod / condition
Resin typeEpoxyAs supplied
Initial viscosity1,200mPa*s77 deg F
Working life50minTime for viscosity to double
Cure temperature176 (80)deg F (deg C)Cure process
Technical properties

After-processing / final-state properties

Values describe cured-system performance and are product-selection data, not specifications.

PropertyValueUnitMethod / condition
Glass transition temperature180 (82)deg F (deg C)Cured system
Flexural strength123MPaCured system
Flexural modulus2.9GPaCured system

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers