LAIRD CR112

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LAIRD CR112

Main features

  • 12-to-18-GHz Absorber Grade
  • Castable Two-Part Epoxy System
  • Molded and Localized RF Absorption

Product Description

Eccosorb CR-112 is a two-part castable epoxy microwave absorber for molding waveguide terminations, attenuators, loads, and custom RF parts or for precisely potting small absorber volumes around RF leakage paths. The system combines Part A resin and Part B catalyst at 100:11.3 by weight. Heating Part A to about 65 deg C improves pourability, and the mixed material has about 30 minutes of pot life at 65 deg C. Recommended cure options range from 1 hour at 150 deg C to 12 hours at 75 deg C. After cure, CR-112 is recommended for the 12 to 18 GHz range.

Key features

  • 12-to-18-GHz absorber grade: The recommended frequency range for CR-112 is 12 to 18 GHz.
  • Two-part castable epoxy: Part A resin and Part B catalyst mix at 100:11.3 by weight.
  • Moldable RF absorption: The liquid system molds terminations, attenuators, loads, and custom RF parts.

Applications

Waveguide terminations, attenuators, loads, molded RF parts, and localized potting around RF leakage paths.

Product Family

LAIRD CR112

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry TypeChemistry Type
Resin: Epoxy
ColorColor
Dark Grey
Density (g)Density (g)
1.60 g/cm3
Thermal Properties
Operating TemperatureOperating Temperature
max 180 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Product-selection data for the exact CR-112 grade; component safety coverage is not represented here.

PropertyValueUnitMethod / condition
Product formTwo-part castable systemPart A resin and Part B catalyst
Resin chemistryEpoxyAs supplied
ColorDark grayTypical; exact CR-112 part page
Mix ratio, Part A:Part B100:11.3by weightCR-112
Minimum shelf life180daysFrom date of shipment; exact part page
Technical properties

After-processing / final-state properties

Values are typical design data for the cured CR-112 material and are not specifications.

PropertyValueUnitMethod / condition
Recommended frequency range12 to 18GHzCR-112
Service temperatureBelow 180deg CCR family; typical
Density1.60g/cm^3Exact CR-112 part page; typical
Linear expansion coefficient30 x 10^-6per deg CTypical
Water absorption0.1%7 days immersion; typical
Flexural strength15,000psiTypical
Outgassing TML / CVCM0.510 / 0.010%Exact CR-112 part page; typical

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers