LAIRD TFLEX 370TG
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Main features
- Cut-Through-Resistant Tgard Barrier
- Mass-Production Part Handling
- Compliant 1.75 mm Gap Filling
Product Description
Tflex 370TG combines a 1.75 mm filled silicone thermal gap-filler sheet with a Tgard carrier liner. The reinforced construction supplies a cut-through-resistant dielectric barrier while improving part handling for mass production. Typical thermal conductivity is 1.2 W/(m K), Shore 00 hardness is 27 and nominal thickness tolerance is +/-10%. Low compression set permits repeated pad use, and the light-green material operates across -40 to 160 deg C. The sheet is adhesive on one side for placement.
Key features
- Tgard dielectric barrier: Adds cut-through resistance to the reinforced sheet.
- 1.75 mm grade thickness: Provides a preformed interface with +/-10% thickness tolerance.
- Production handling: The carrier liner supports easier part handling in mass production.
Applications
Applications include telecom hardware, flat panels, memory modules, power conversion, automotive electronics, LED lighting and handheld electronics.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Values describe the supplied preformed sheet before installation.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Construction | Filled silicone elastomer on carrier liner | Typical | |
| Reinforcement carrier | Tgard | Exact family construction | |
| Color | Light green | Visual | |
| Nominal thickness | 1.75 | mm | Exact grade |
| Thickness tolerance | +/-10 | % | Typical |
| Specific gravity | 1.79 | ASTM D792 | |
| Hardness | 27 | Shore 00 | ASTM D2240 |
| Shelf life | 2 | years | From date of shipment |
After-processing / final-state properties
Values describe bulk or compressed material under the stated test conditions, not complete assembly performance.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Thermal conductivity | 1.2 | W/(m K) | ASTM D5470; typical |
| Thermal resistance | 1.59 | deg C in^2/W | At 10 psi; ASTM D5470 modified |
| Coefficient of thermal expansion | 600 | ppm/deg C | IPC-TM-650 2.4.24 |
| Operating temperature | -40 to 160 | deg C | Typical range |
| Breakdown voltage | More than 10,000 | VAC | ASTM D149 |
| Flammability rating | 94V0 | UL |