BCP-1522 | Medium voltage Busbar Coating Powder
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- Low and medium voltage applications
- Suitable for applications up to 38 kV
- Optimized for fluidized bed coating process
Product Description
LINQSOL BCP-1522 is a thermosetting coating powder designed for low to medium-voltage busbar and switchgear applications. Once cured, BCP-1522 forms a smooth, durable, and moisture-resistant coating, suitable for operations up to 38 KV. The powder allows for fast and significant coating buildup, which speeds up production cycles. It can be used effectively on both copper and aluminum busbars, creating coatings that are over 200 mil (5 mm) thick.
LINQSOL BCP-1522 also boasts a high UL746B Relative Thermal Index (130 °C), ensuring reliable performance even under elevated temperatures. Its fine particle size (44–210 µm), which is optimized for fluidized bed coating systems, promotes uniform application and consistent coating quality.
Advantages of BCP-1522 for Busbar Coating
- Suitable for copper and aluminum bar
- Smooth, uniform coating build in excess of 200 mils (5 mm)
- Rapid build rates to reduce cycle times
- Fine grind powder to replenish size distribution
- Fluidizing agent to promote uniform build
- Ongoing testing to optimize quality & productivity
Typical applications and uses of BCP-1522 include:
- Low Voltage (600V) Copper, Aluminum and Brass Busbars
- Medium Voltage (up to 38kV) Copper, Aluminum and Brass Busbars
- Switchgear Equipment for Power Distribution
Recommended coating Temperature:
- 170 – 220 °C. (170 °C x 20 min or 210 °C x 5 min )
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Other Properties
Mechanical Properties
Additional Information
Storage and Handling
Powder should be stored at 10°C or below, in closed containers. After removal from cold storage, the material must be allowed to come to room temperature in the sealed container to avoid moisture contamination. The suggested waiting time is 24 hours. Please consult our Product Handling Recommendations for Coating Powders. For safe handling information on this product, consult the Material Safety Data Sheet (MSDS).