Main features

  • Low viscosity
  • Good workability
  • High temperature resistance

Product Description

OPTOLINQ OLS-1557 is an optically clear, two-part, and heat-curable epoxy resin. OLS-1557 AB mixture has low viscosity and good workability after mixing. When fully cured, the product demonstrates minimal mold shrinkage, high toughness, high-temperature resistance, good adhesion on different surfaces, and excellent electrical properties, making OLS-1557 an ideal material for the encapsulation of optoelectronic devices. 

 

Product Family

LINQ OLS-1557

1. Select Package Type
2. Select Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type and Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
4 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
81–91 °C
Chemical Properties
Water AbsorptionWater Absorption
0.3 %

Additional Information

Processing Instructions

  • Mix component A and B, stir uniformly, and degas under vacuum. 
  • Recommended molding curing conditions: Mold at 150 °C for 5 minutes and post-mold cure at 130–135 °C for 6–8 hours. Identify the specific curing settings based on your product requirements.

Using Additives

Optolinq OLS-1557 can be mixed with diffusing agents or color pastes to achieve customer-specific purposes.

Recommended quantity of various diffusing agents and color pastes:

  • OPC-R Red Color Paste: 0.1-0.5% by epoxy weight
  • OPC-B Blue Color Paste: 0.1-0.5% by epoxy weight
  • OPC-G Green Color Paste: 0.1-0.5% by epoxy weight
  • ODF-090 Diffusing Agent: 3-5% by weight (LED lamps), 4-8% (LED displays)

Storage and Handling

Store in a ventilated, dry, and clean environment below 30 °C and  70% RH. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, Part A has a shelf life of 6 months and Part B a shelf life of 3 months. Shelf life can be extended by using cold storage.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers