PIT1A-ESD | 1mil Antistatic ESD Polyimide (Kapton) Tape with Acrylic Adhesive
Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

Main features
- 1 mil polyimide film
- Acrylic adhesive
- >6000V breakdown voltage
Product Description
LINQTAPE™ PIT1A-ESD Series is a high-temperature resistant, antistatic-treated polyimide film mounted with an acrylic adhesive. It is designed for both masking and temporary bonding in many high-temperature applications in semiconductor, electronic, automotive, and other general manufacturing industries.
LINQTAPE™ PIT1A-ESD Series provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It has enhanced strength for puncture and tear resistance and can be used in applications that may see intermittent temperatures up to 155°C (311°F).
LINQTAPE™ PIT1A-ESD Series comes as a standard in 36-yard (33m) lengths of varying widths, but longer rolls may be available upon request. Please note that batches after April 2024 will all come with a release liner.
Key Features:
- Antistatic coating to dissipate electrostatic charge
- Pressure-sensitive acrylic adhesive
- Excellent insulating properties
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Other Properties
Mechanical Properties
Additional Information
Application Ideas
- Dissipate electrostatic charges
- Protection of static-sensitive devices
- Temporary bonding of thermocouples for oven profiling
- Bonding of devices before solder reflow
- Splicing of insulation layers