PIT2A-LO | 2-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT2A-LO | 2-mil Polyimide (Kapton) Tape with Low Outgassing Acrylic Adhesive

Main features

  • 2 mil polyimide film
  • Non-silicone, low outgassing acrylic adhesive
  • 6,500 V breakdown voltage

Product Description

LINQTAPE™ PIT2A-LO is a Polyimide tape with 2mil backing thickness and 1.5mil acrylic adhesive with low outgassing. This tape has less than 1% TML and less than 0.1% CVCM values, making it suitable for aerospace applications. 

LINQTAPE™ PIT2A-LO has good adhesion and tensile strength and can operate in temperatures between -29°C to 177°C.

Product Family

LINQ PIT2A-LO

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Temperature ResistanceTemperature Resistance
177 ˚C
Electrical Properties
Breakdown VoltageBreakdown Voltage
6,500 V
Mechanical Properties
Adhesion StrengthAdhesion Strength
50 Oz/in
ElongationElongation
55 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
88 N/cm
General Properties
Adhesive LayerAdhesive Layer
Low Outgassing Acrylic
Adhesive ThicknessAdhesive Thickness
38.1 µm
ColorColor
Amber
Film ThicknessFilm Thickness
50.8 µm
Release LinerRelease Liner
Paper
Total ThicknessTotal Thickness
88.9 μm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers