PIT5S-RL | 5-mil Polyimide (Kapton) Tape with Silicone Adhesive & Release liner

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT5S-RL | 5-mil Polyimide (Kapton) Tape with Silicone Adhesive & Release liner

Main features

  • 5 mil polyimide film
  • Silicone adhesive
  • >18000V breakdown voltage

Product Description

LINQTAPE™ PIT5S-RL is a high performance, high-temperature resistant, pressure sensitive polyimide tape designed for permanent bonding in many high temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive and general manufacturing industries.

LINQTAPE™ PIT5S-RL provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 260°C (500°F).

LINQTAPE™ PIT5S-RL comes in 33 meter (36 yard) length rolls of varying widths. The base polyimide film (backing) thickness is 5 mil (127 ± 2µm) thick and the total thickness including the adhesive layer is approximately 7 mil (177.8 ± 6µm). The only difference with the plain version is that this product comes on a release liner.

Product Family

LINQ PIT5S-RL

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Silicone
Adhesive ThicknessAdhesive Thickness
38.1 µm
Chemistry TypeChemistry Type
Polyimide
ColorColor
Amber
Film ThicknessFilm Thickness
127 µm
Release LinerRelease Liner
Yes
Single or Double-Sided AdhesiveSingle or Double-Sided Adhesive
Single
Special LayerSpecial Layer
None
Total ThicknessTotal Thickness
165.1 μm
Thermal Properties
Temperature ResistanceTemperature Resistance
260 ˚C
Electrical Properties
Breakdown VoltageBreakdown Voltage
>18000 V
Dielectric StrengthDielectric Strength
118 kV/mm
Volume ResistivityVolume Resistivity
10000000000000 Ohms⋅cm
Other Properties
RoHS CompliantRoHS Compliant
Yes
VOC-Free (100% solids content)VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion StrengthAdhesion Strength
25 Oz/in
ElongationElongation
65 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
172 N/cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers