TPP500 | 500um Sintered Titanium Powder

Harmonization Code : 81089090 | Titanium and articles thereof, including waste and scrap other: other

TPP500 | 500um Sintered Titanium Powder

Main features

  • 0.50mm - 500um - 20mil
  • 30–40% Porosity
  • Gas Diffusion and Porous Transport Layer for PEM Water Electrolyzers and Fuel Cells

Product Description

LINQCELL TPP500 is a 0.50-mm thick, porous sintered sheet made from Grade 1 titanium powders. It is formed by cold isostatic pressing followed by high-temperature vacuum sintering. The cold forming process uses no additional adhesives, ensuring that the product maintains high purity and does not contain phases that could affect the electrical properties of the sintered material.

Similar to sintered titanium fiber felts, LINQCELL TPP500 sintered titanium powder offers high electrical conductivity, corrosion resistance in harsh, low pH environments, and high mechanical strength. However, it is denser and has lower porosity, typically less than 50%, compared to sintered titanium fibers. This higher density results in greater strength.

Key Features:

  • High corrosion resistance even under acidic conditions
  • High electrical conductivity
  • Low porosity (30–40%) perfect for water electrolyzer stacks
  • Higher mechanical strength than those of sintered titanium fiber felts

Titanium is an ideal material for porous transport layer (PTL) fabrication due to its ability to withstand the corrosive environment of the oxygen evolution reaction while providing effective electrical conductivity. The porous structure of these plates enables efficient gas diffusion and electrolyte distribution, minimizing mass transport losses.

Highly Recommended for:

Product Family

LINQ TPP500

1. Select Sheet Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Sheet Size.

Technical Specifications

General Properties
Total ThicknessTotal Thickness
500 μm

Additional Information

Sintered metal powder is a porous material produced by sintering, a process wherein the metallic powder is compressed and then heated at temperatures below its melting point. Sintering causes the particles to bond into a solid piece with small pores. Typically, sintered metal powders have a high solid volume fraction, ranging from 0.35 to 0.65; thus, this type of porous material is commonly used in applications where good mechanical strength is required.

Manufacturing Sintered Metal Powders



Sintered metal powders are formed by sintering compacted powders. Sintering is the key step in the production of both sintered metal powders and sintered metal fibers. It is a manufacturing process where metal raw materials are heated to high temperatures, just below their melting point. This causes the particles to fuse together, forming a solid mass. During sintering, several changes occur in the metal powder particles, improving various properties like strength, ductility, corrosion resistance, conductivity, and magnetic permeability. These changes are vital for different applications, as they determine the material's porosity, strength, and overall performance. Therefore, sintering plays a major role in achieving the properties needed for specific uses.


Reference: Samal, Prasan K. Newkirk, Joseph W.. (2015). ASM Handbook, Volume 07 - Powder Metallurgy (2015) - 34.2 Improved Mechanical Properties.(pp. 332). ASM International.

Variation in Compact Properties with Degree of Sintering 

Variation in Compact Properties with Degree of Sintering 

Sintering Mechanism in Metal Powders

Different Stages of Sintering

The different sintering stages show how loose metal powders transform into a solid object:

First Sintering Stage

At the initial stage of sintering, particles start sticking together due to weak forces, like van der Waals' forces. At higher temperatures, they rearrange and pack together, sometimes rotating and twisting to achieve lower energy states in terms of their arrangement.

 

Neck Formation during Sintering
In the next stage, a sinter bond begins to form between the contact points established earlier, forming necks between particles. This occurs because atoms move from the surface of the particles to the contact points, reducing the surface area and forming interparticle bonds. This process, driven by surface transport mechanisms, strengthens the connections between particles but does not reduce the distance between them. Although this marks the start of sintering, there is little to no significant densification yet.

 

Neck Growth and Densification during Sintering

This stage is followed by the intermediate stage, where neck growth occurs, leading to densification. During this phase, the necks lose their distinct identities, and the pores become rounded but remain interconnected. At this point, the centers of the two spheres start to get closer, resulting in shrinkage. Bulk transport mechanisms predominate, facilitating neck growth and the elimination of pores. 

In the final stage of sintering, interconnected open pores close and turn into isolated closed pores. As this happens, grain growth occurs, which slows down the surface and bulk diffusion processes. Consequently, this stage becomes the slowest, as densification increases from 95% to 99%.

(SD: Surface Diffusion, VD: Vacancy Diffusion, GB: Grain Boundary Diffusion)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers