LINQBOND GT2301 | Glob Top

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LINQBOND GT2301 | Glob Top

Main features

  • solvent-free
  • excellent vibration resistance
  • one-component

Product Description

LINQBOND GT2301 is a one-component epoxy adhesive designed for electronic device applications. It forms tough, strong structural bonds that provide excellent shear, peel, and impact strength.

LINQBOND GT230 is suitable for the encapsulation of electronic products. Its durability is exceptional, and it can pass numerous environmental tests.

Product Family

LINQBOND GT2301

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 16 weeks
CA Shipping in 16 weeks
EU Shipping in 16 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
7 hours
Specific GravitySpecific Gravity
1.48
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
130 °C
Electrical Properties
Surface ResistivitySurface Resistivity
4.5E14 Ohms/sq
Volume ResistivityVolume Resistivity
4.5E15 Ohms⋅cm
Chemical Properties
Water AbsorptionWater Absorption
0.58 %
Physical Properties
ViscosityViscosity
45000-85000 mPa.s

Additional Information

Instructions for Use:

  1. Before use, thaw the product to reach room temperature for 1–2 hours. Syringe should be placed vertically while thawing. Keep container airtight until room temperature is reached.

  2. Ensure the surface to be bonded is clean and free of contaminants like dirt, grease, or mold release agents. A simple solvent wipe is often sufficient.

  3. Cure time may vary based on the actual part geometry, material volume, and equipment. It is recommended to test on actual parts and equipment.

  4. For large-scale applications, consider a staged curing process: start with a lower temperature precure, followed by a full cure at a higher temperature to effectively manage heat release.

  5. The epoxy cannot be refrozen once exposed to room temperature.

 

Storage and Handling


Store and transport at a -5°C temperature. Keep away from moisture and heat sources. It is strictly forbidden to store in outdoor environments. Lower temperatures will ensure better flow and nullify any chance of cross-linking.

 

  • Shelf life at -5°C  is 365 days.

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers