LOCTITE 190828

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

LOCTITE 190828

Main features

  • Rapid Humidity-Cure Bonding
  • Thermal-Cycling-Resistant Cyanoacrylate Adhesion
  • Multi-Substrate Instant Assembly

Product Description

LOCTITE 190828 is a one-part clear cyanoacrylate instant adhesive that cures with humidity. The uncured liquid has a typical viscosity of 613 mPa s at 25 deg C, measured with a Brookfield LVF viscometer using spindle 2 at 30 rpm. It develops high handling strength rapidly after bonding and is formulated for thermal-cycling resistance. A 365-day shelf life applies when stored at 2 to 8 deg C in the unopened container. Applications include rapid bonding of metals, plastics, and elastomers.

Key features

  • Brookfield viscosity: Typical viscosity is 613 mPa s at 25 deg C.
  • Rapid humidity cure: The adhesive develops high handling strength rapidly after bonding.
  • Thermal-cycling resistance: The cyanoacrylate is formulated for thermal-cycling resistance.

Applications

Applications include rapid bonding of metals, plastics, and elastomers.

Product Family

LOCTITE 190828

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear liquid
Physical Properties
ViscosityViscosity
613 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear liquid-As supplied
Viscosity613mPa sTypical; 25 deg C; Brookfield LVF, spindle 2, 30 rpm
Shelf life365daysUnopened container; 2 to 8 deg C
Optimal storage2 to 8deg CUnopened container in a dry location

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers