LOCTITE 2892
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

Main features
- High-Viscosity Flange Gap Filling
- Resilient Flange-Movement Sealing
- Manual or Screen-Print Application
Product Description
LOCTITE 2892 is a one-component, blue, high-viscosity anaerobic methacrylate sealant for form-in-place sealing between rigid metal flanges. It fills surface imperfections and has a stated gap-filling capability up to 0.254 mm, while application directions specify close-fitting flange gaps up to 0.1 mm. Brookfield viscosity is 2,500,000 to 4,600,000 mPa s at 0.5 rpm and 450,000 to 950,000 mPa s at 5 rpm, both at 25 deg C. After cure between mating flanges, it forms a tough, resilient seal that flexes with movement from vibration, pressurization, or thermal changes. Application methods include a continuous manual bead or screen printing.
Key features
- Close-flange gap filling: Gap-filling capability extends to 0.254 mm, while application directions specify close-fitting flanges with gaps up to 0.1 mm.
- High-viscosity rheology: Brookfield viscosity spans 2,500,000 to 4,600,000 mPa s at 0.5 rpm and 450,000 to 950,000 mPa s at 5 rpm.
- Resilient cured seal: The cured material flexes with flange movement caused by vibration, pressurization, or thermal changes.
Applications
Applications include form-in-place sealing of close-fitting rigid metal flanges by continuous manual bead or screen printing.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Blue viscous material | Uncured material; LMS | |
| Specific gravity | 1.1 | At 25 deg C | |
| Viscosity | 2,500,000 to 4,600,000 | mPa s (cP) | LMS; Brookfield HBT; spindle TC; 0.5 rpm; Helipath; 25 deg C |
| Viscosity | 450,000 to 950,000 | mPa s (cP) | LMS; Brookfield HBT; spindle TC; 5.0 rpm; Helipath; 25 deg C |
| Gap-filling capability | Up to 0.254 | mm | Product characteristic |
| Close-fitting flange gap | Up to 0.1 | mm | Application directions |