LOCTITE 3296 | UV-curable Epoxy Adhesive

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE 3296 | UV-curable Epoxy Adhesive

Main features

  • Fast UV cure
  • High Tg and low CTE
  • Low shrinkage during & after cure

Product Description

LOCTITE® 3296 is a dual-cure adhesive specifically developed for Automotive ADAS Optical Modules, including critical bonding applications like lens barrel-to-housing and lens housing-to-circuit board assemblies. This advanced adhesive is engineered for high-performance environments where precise alignment and long-term stability are essential. With a fast UV cure that can achieve primary bonding in as little as 3 seconds under adequate UV exposure, LOCTITE® 3296 significantly speeds up production cycles, reducing downtime and increasing throughput. Its exceptional thermal stability is highlighted by a Glass Transition Temperature (Tg) of 189°C, making it ideal for components exposed to intense heat. Its low Coefficient of Thermal Expansion (CTE) of 22.1 ppm/°C (between 25-125°C) and minimal shrinkage of 0.3% ensure that it maintains a strong, reliable bond even in demanding thermal conditions, minimizing the risk of component stress or misalignment over time.

Mechanically, LOCTITE® 3296 provides robust support with a Shore D hardness of 94 and an E-Modulus of 10,900 MPa at 25°C, offering excellent stiffness and durability for critical assemblies. This makes it particularly suited for optical modules where precise bonding is crucial for long-term optical clarity and alignment. LOCTITE® 3296 is well-suited for automated production environments, exhibiting low-viscosity behavior that ensures smooth, consistent dispensing. It is also designed to work without SVHCs and antimony, aligning with industry demands for environmentally responsible manufacturing processes.

Product Family

LOCTITE 3296

1. Select Package Type
2. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 38 days
CA Shipping in 8 weeks
EU Shipping in 25 days
Packaging
Please select Package Type and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)Density (g)
1.8 g/cm3
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
189 °C
Physical Properties
ViscosityViscosity
33,700 mPa.s
Young's modulusYoung's modulus
10,900 MPa

Additional Information

LOCTITE 3296 Additional Technical Specifications

Property Value Unit
Shear thinning index 4.3 1.5/15s-1
Cure Shrinkage, Linear 0.33 %
Cure Depth (UV Only) >3 mm

Conditioning

  • Allow container to reach room temperature before use.

Thawing Directions

  • 30/55cc: 1 hour
  • 6oz: 2 hours

Required UV Cure

  • Light Source and Condition: UV LED
  • UV Wavelength: 365 nm
  • Irradiance at Bond Line: 1,000 mW/cm2
  • Recommended Time: 3 seconds

Recommended Heat Cure

  • 30 minutes @120℃
  • 60 minutes @100℃

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers