LOCTITE 3515

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE 3515

Main features

  • Cornerbond
  • Fast cure
  • Self alignment of SMT components

Product Description

LOCTITE 3515 is a one component epoxy adhesive, designed to allow self-alignment of SMT components during the reflow operation. The adhesive is pre-applied to the board at the corners of the CSP pad site using a standard SMA dispenser, a process that speeds assembly by eliminating post-reflow underfill dispense and cure steps.

LOCTITE 3515 cures during the solder reflow phase to form a reliable bond, and contributes to improvements in handheld device reliability. LOCTITE 3515 cornerbond has excellent dispensing characteristics, good dot profile, and good on-board electrical characteristics. Reinforcement of CSPs with interposers or comerless arrays in portable electronic devices.

Cure Schedule

  • 30 minutes @ 150 °C
  • 5 minutes @ 180 °C
  • 30 seconds @ 200 °C
  • 15 seconds @ 220 °C
Product Family

LOCTITE 3515

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 29 days
CA No longer available
EU Shipping in 20 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.23
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
73 °C
Thermal ConductivityThermal Conductivity
0.28 W/m.K

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers