LOCTITE 3619

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE 3619

Main features

  • SMD components on PCB
  • Chipbonder
  • Very High dispense speed

Product Description

LOCTITE 3619 is designed for bonding of surface mounted devices to printed circuit boards prior to wave soldering. Particularly suited where low curing temperatures arerequired with heat sensitive components, and in applications where short curing times are required.

LOCTITE 3619 is a red, high viscosity, epoxy paste with high wet strength. It claims 25,000 - 40,000 dots per hour dispensing speed and is typically used for mountin SMD components onto a PCB.

Cure schedule

  • 30 minutes @ 100°C 

Note: Sufficient time must be added to allow the bond location to reach the desired cure temperature. Curing profiles should be developed for each device. Bond strength achieved in practice will vary considerably depending on the SMD component type, adhesive dot size and the type, grade and degree of cure of the solder mask/resist.

Product Family

LOCTITE 3619

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.22
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
50 °C
Electrical Properties
Volume ResistivityVolume Resistivity
1200000000000000 Ohms⋅cm
Physical Properties
ViscosityViscosity
3,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers