LOCTITE 50H
Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

Main features
- Low-Viscosity Instant Bonding
- Colorless Assembly Bonding
- Fast Dissimilar-Substrate Bonding
Product Description
LOCTITE 50H is a one-part ethyl cyanoacrylate instant adhesive for rapid bonding of plastics and compatible dissimilar substrates. This colorless liquid has a typical viscosity of 15 to 40 cP and a specific gravity of 1.06, placing its as-supplied behavior in a low-viscosity range. Its cured profile includes thermal, dielectric and bond-performance characteristics for evaluating supported assemblies. The listed configuration is supplied as a 500 g cartridge. Applications include fast bonding of plastics and other compatible dissimilar materials.
Key features
- Low-viscosity grade: Typical viscosity is 15 to 40 cP.
- Colorless liquid: The supplied adhesive is a colorless liquid with specific gravity of 1.06.
- Dissimilar-material bonding: Applications include plastics and other compatible dissimilar materials.
Applications
Fast bonding of plastics and other compatible dissimilar materials.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Curing Conditions
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Colorless liquid | As supplied | |
| Specific gravity | 1.06 | As supplied | |
| Viscosity | 15 to 40 | cP | Typical; exact product technical data |