LOCTITE 5452

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

LOCTITE 5452

Main features

  • Particle-Free Hydraulic Sealing
  • Large-Diameter Thread Coverage
  • Hand-Tool Fitting Disassembly

Product Description

LOCTITE 5452 is a one-part, purple methacrylate ester thread sealant for hydraulic and pneumatic fittings. The medium-viscosity, thixotropic liquid cures anaerobically when confined between close-fitting metal threads. It is formulated without fillers or particles that could interfere with hydraulic systems and is suited to tapered and large-diameter pipe, dry-seal, O-ring boss, and flare-style fittings. On flare fittings, the sealant can cover scratches and surface imperfections on mating faces. Cured fittings can normally be disassembled with standard hand tools, with mechanical cleaning before reuse.

Key features

  • Particle-free formulation: Contains no fillers or particles that could interfere with a hydraulic system.
  • Multiple fitting geometries: Applies to tapered pipe, dry-seal, O-ring boss, and flare-style fittings.
  • Anaerobic metal-thread cure: Cures when confined without air between close-fitting metal threads.

Applications

Applications include sealing hydraulic and pneumatic threaded fittings, including tapered and large-diameter pipe, dry-seal, O-ring boss, and flare fittings.

Product Family

LOCTITE 5452

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Purple liquid
Chemistry TypeChemistry Type
Methacrylate ester
Specific GravitySpecific Gravity
1.15
Physical Properties
ViscosityViscosity
15,000 to 40,000 mPa.s
Other Properties
Storage TemperatureStorage Temperature
8°C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Specific gravity1.15-Typical at 25 deg C
Viscosity15,000 to 40,000mPa s (cP)Specification range; Brookfield RVT, spindle 6, 25 deg C, 20 rpm
Viscosity2,500 to 6,500mPa s (cP)Specification range; cone and plate, Physica MK22, cone CP50-1, 25 deg C, shear rate 20 s^-1
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Breakaway torque0.9N mTypical; ISO 10964, unseated degreased 3/8 x 16 steel nuts and bolts, after 1 hour at 22 deg C
Compressive shear strength>=1.7N/mm^2Specification minimum; ISO 10123, degreased steel pins and collars, after 24 hours at 22 deg C
Breakaway torque3.5N mTypical; ISO 10964, unseated degreased 3/8 x 16 steel nuts and bolts, after 24 hours at 22 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers