LOCTITE 5607F
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- Fluorescent Part B Identification
- Two-Part Metered Mixing
- SI 5607 Hardener Component
Product Description
LOCTITE SI 5607F is the fluorescent Part B hardener component used in the LOCTITE SI 5607 two-part silicone system. The component is supplied as a gray paste, with a typical specific gravity of 1.6 to 1.8 at 25 deg C. Typical cone-and-plate viscosity is 20,000 to 35,000 mPa s at 25 deg C and a shear rate of 20 s^-1. Combine this Part B hardener with Part A to form the LOCTITE SI 5607 system. The cured system's bonding, sealing, mechanical, and electrical properties do not apply to LOCTITE SI 5607F alone.
Key features
- Fluorescent component identification: Fluorescent Part B hardener for the LOCTITE SI 5607 system.
- Part B viscosity: Typical cone-and-plate viscosity is 20,000 to 35,000 mPa s at 25 deg C and 20 s^-1.
- Part B specific gravity: Typical specific gravity is 1.6 to 1.8 at 25 deg C for the Part B hardener.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
As-supplied properties
Values apply to the LOCTITE SI 5607 Part B hardener component only.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Gray paste | - | Part B; as supplied |
| Specific gravity | 1.6 to 1.8 | - | Typical; Part B; 25 deg C |
| Viscosity | 20,000 to 35,000 | mPa s | Typical; Part B; cone and plate; 25 deg C; shear rate 20 s^-1 |