Main features

  • High-Temperature Steam Thread Sealing
  • High-Pressure Steel Joint Sealing
  • Medium-Strength Anaerobic Locking

Product Description

LOCTITE 5770 is a high-temperature, medium-strength anaerobic dimethacrylate sealant for metal threaded pipes and fittings in industrial service. Its high-viscosity thixotropic paste is particularly suited to steel joints requiring both high-temperature and high-pressure resistance. At 25 deg C, typical specific gravity is 1.27 and typical cone-and-plate viscosity is 30,000 to 90,000 mPa s at 50 s^-1. Typical removal torque after 72 hours at 22 deg C is 74 N m on 3/8 in malleable iron tees and steel plugs pre-torqued to 27 N m. The product also sealed 100 psi air after a 5-minute cure in an ASTM D6396 fitting test and has been tested for steam resistance at temperatures up to 280 deg C.

Key features

  • High-temperature steel sealing: Designed for steel threaded joints where high-temperature and high-pressure resistance is required.
  • Early-cure pressure sealability: 3/8 in NPT malleable iron tees and steel plugs sealed 100 psi air after 5 minutes of cure at 22 deg C in an ASTM D6396 test.
  • High-temperature steam testing: Forged-steel NPT steam assemblies were tested at temperatures up to 280 deg C and pressures up to 6.4 MPa.

Applications

Sealing metal threaded pipes and fittings, including industrial steam service.

Product Family

LOCTITE 5770

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Off-white to purplish gray paste
Chemistry TypeChemistry Type
Dimethacrylate ester
Specific GravitySpecific Gravity
1.27
Physical Properties
ViscosityViscosity
30,000 to 90,000 mPa.s
Other Properties
Storage TemperatureStorage Temperature
8°C to 21 °C

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
AppearanceOff-white to purplish gray paste-Uncured
Specific gravity1.27-Typical; 25 deg C
Viscosity30,000 to 90,000mPa sTypical; cone and plate; 25 deg C; 50 mm parallel plates; 0.5 mm gap; 50 s^-1
Technical properties

Cured properties and performance

PropertyValueUnitMethod / condition
Breakloose torque9.0 to 28.4N mTypical; ISO 10964; after 24 h at 25 deg C; 3/8 x 16 grade 5 steel nuts and bolts; degreased; pre-torqued to 5 N m
Removal torque74N mTypical; ASTM D6396; after 72 h at 22 deg C; 3/8 in malleable iron tees and steel plugs; pre-torqued to 27 N m
Air pressure sealability100psiASTM D6396; 3/8 in NPT malleable iron tees and steel plugs; pre-torqued to 27 N m; cured 5 min at 22 deg C
Steam weight loss0%ASTM D6396-based steam test; 232 deg C; 2.9 MPa; 48 h; cured 24 h at 22 deg C plus 2 h at 150 deg C
Steam weight loss4%ASTM D6396-based steam test; 280 deg C; 6.4 MPa; 48 h; cured 24 h at 22 deg C plus 2 h at 150 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers