LOCTITE CAT 28
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- Low-Viscosity Catalyst Handling
- Long-Pot-Life System Processing
- STYCAST 2651MM Catalyst Pairing
Product Description
LOCTITE CAT 28 is the Part B epoxy cure catalyst used with LOCTITE STYCAST 2651MM for encapsulation; it is not the complete encapsulant. The catalyst has a typical viscosity of 275 mPa s at 25 deg C and density of 1.05 g/cm^3. In the STYCAST 2651MM system, the material-to-catalyst mix ratio is 100:12 by weight or 100:18.5 by volume. CAT 28 provides heat cure and long pot life when used with STYCAST 2651MM.
Key features
- Low-Viscosity Catalyst: Typical CAT 28 viscosity is 275 mPa s at 25 deg C.
- Long Pot Life: For heat-cured encapsulation with STYCAST 2651MM.
- STYCAST 2651MM Mix Ratios: STYCAST 2651MM uses CAT 28 at 100:12 by weight or 100:18.5 by volume.
Applications
Catalyst component used with LOCTITE STYCAST 2651MM for encapsulation.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
CAT 28 is Part B only; mix ratios refer to the STYCAST 2651MM material-to-catalyst system.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Viscosity | 275 | mPa s | Typical CAT 28 at 25 deg C |
| Density | 1.05 | g/cm^3 | Typical CAT 28 |
| Material:catalyst mix ratio by weight | 100:12 | STYCAST 2651MM:CAT 28 system | |
| Material:catalyst mix ratio by volume | 100:18.5 | STYCAST 2651MM:CAT 28 system |