LOCTITE EA 3501HT

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 3501HT

Main features

  • Paint-Bake Seam Sealing
  • Zero-Sag Epoxy Paste
  • No-Mix One-Component Processing

Product Description

LOCTITE EA 3501HT is a one-component heat-cure epoxy seam sealant designed for primed, bare or oily metal surfaces processed through high-temperature paint-bake operations. The gray high-viscosity paste requires no component mixing and has typical vertical and horizontal sag of 0 mm under SAE J2433, Method B. The recommended 30-minute cycle uses a minimum cure temperature of 160 deg C, a typical temperature of 175 deg C and a maximum of 225 deg C. After cure, the sealant remains flexible and is used on welded or bonded seams, overlap joints, butt joints and visible seams in automotive and industrial metal assemblies.

Key features

  • No-Mix Heat Cure: One-component epoxy paste uses a 30-minute paint-bake cure cycle, with a typical cure temperature of 175 deg C, a minimum of 160 deg C and a maximum of 225 deg C.
  • Non-Sag Paste: Typical vertical and horizontal sag are both 0 mm under SAE J2433, Method B.
  • Paint-bake seam sealing: Designed for primed, bare or oily metal seams processed through high-temperature paint-bake operations.

Applications

Sealing automotive and industrial metal seams, overlap joints and butt joints where heat cure through a paint-bake process is used.

Product Family

LOCTITE EA 3501HT

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Grey paste
Chemistry TypeChemistry Type
Epoxy
SolidsSolids
100 %
Specific GravitySpecific Gravity
1.35
Physical Properties
ViscosityViscosity
480,000 mPa.s
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
30 °C
Other Properties
Storage TemperatureStorage Temperature
2 to 25 °C

Additional Information

Technical properties

As-supplied properties

PropertyValueUnitMethod / condition
Specific gravity1.3523 deg C; ASTM D927
Viscosity480,000mPa sCP25-2 oscillation; 25 deg C
Solids content100%ASTM D2834
Vertical sag0mmSAE J243
Horizontal sag0mmSAE J243
Minimum cure30min160 deg C
Typical cure30min175 deg C
Maximum cure30min225 deg C
Technical properties

Final-state properties

PropertyValueUnitMethod / condition
Hardness75Shore ACured 30 min at 175 deg C
Glass transition temperature30deg CISO 11359-2; cured state
Low-temperature mandrel bendNo cracking or adhesion loss-40 deg C; SAE J1243 Method B; 50 mm diameter
Tensile modulus9.7N/mm^2ISO 527-3; cured state
Tensile strength2.4N/mm^2ISO 37; cured state

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers