LOCTITE EA 9035

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA 9035

Main features

  • Rapid Four-Minute Repair Window
  • Non-Sag Vertical Placement
  • Equal-Part 1:1 Cartridge Mixing

Product Description

LOCTITE EA 9035 is a cartridge-based, two-part clear epoxy adhesive for general-purpose rapid bonding and repair. It uses a 1:1 mix ratio, has a 4-minute work life, and sets in approximately 5 minutes. The gel consistency provides non-sag behavior on vertical surfaces, keeping the material in place during short repair and assembly operations. The combination of rapid set, equal-part mixing, and vertical application behavior makes this epoxy useful for general repair work where a brief working window is required.

Key features

  • Rapid-Repair Working Window: Work life is 4 minutes for rapid bonding and repair operations.
  • Non-Sag Gel: Gel consistency provides non-sag behavior on vertical surfaces.
  • Equal-Part Epoxy Mixing: The two components use a 1:1 mix ratio.

Applications

General-purpose rapid bonding and repair.

Product Family

LOCTITE EA 9035

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two Part (Resin | Hardener)
Mix RatioMix Ratio
1:1

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers