Loctite EA 9360 AERO Epoxy Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite EA 9360 AERO Epoxy Adhesive

Main features

  • Toughened Structural Epoxy Bonding
  • 50-Minute Assembly Pot Life
  • Room-Temperature Aircraft Bonding Cure

Product Description

LOCTITE® EA 9360 AERO is a two-component, toughened epoxy paste adhesive that cures at room temperature and combines high room-temperature peel strength with tensile lap shear performance at elevated temperatures. Its low-slump consistency supports controlled application, while the 50-minute pot life at 77°F (25°C), 200 g mass, provides time for mixing and assembly. The adhesive develops handling strength after 24 hours at 77°F (25°C) and reaches normal performance after a 5–7 day room-temperature cure. Accelerated curing may be used for small masses, including 1 hour at 180°F (82°C). It is also available in dual-cartridge packaging for two-component dispensing.

Key features

  • High peel strength: Delivers a typical floating-roller peel strength of 68 lb/in (303 N/25 mm) after 7 days at 77°F (25°C) on prepared and primed 2024-T3 AlClad aluminum.
  • Elevated-temperature bond performance: Retains typical tensile lap shear strength of 2,000 psi (13.8 MPa) at 225°F (107°C) on phosphoric-acid-anodized 2024-T3 bare aluminum.
  • Room-temperature or accelerated cure: Reaches normal performance after 5–7 days at 77°F (25°C), with accelerated cures up to 200°F (93°C) available for small adhesive masses.
Product Family

LOCTITE EA 9360

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two Part (A/B)
Mechanical Properties
ElongationElongation
5 %
Thermal Properties
Thermal ConductivityThermal Conductivity
0.25 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical uncured, mixing, working-time, storage and cure information for LOCTITE® EA 9360 AERO. Component and mixed-material values are identified separately.

Property Value Unit Method / condition
Product type Two-component toughened epoxy paste adhesive — Requires mixing before application
Color — Part A Off-white — Unmixed component
Color — Part B Blue — Unmixed component
Viscosity — Part A 3,000 Poise 77°F; Brookfield HBT, spindle 7 at 20 rpm
Viscosity — Part B 1,700 Poise 77°F; Brookfield HBT, spindle 6 at 20 rpm
Viscosity — Mixed 1,200 Poise 77°F; Brookfield HBT, spindle 5 at 20 rpm
Viscosity — Part A 300 Pa·s 25°C; Brookfield HBT at 2.1 rad/s
Viscosity — Part B 170 Pa·s 25°C; Brookfield HBT at 2.1 rad/s
Viscosity — Mixed 120 Pa·s 25°C; Brookfield HBT at 2.1 rad/s
Density — Part A 1.16 g/mL Unmixed component
Density — Part B 1.00 g/mL Unmixed component
Density — Mixed 1.14 g/mL Mixed adhesive
Mix ratio by weight — Part A:Part B 100:43 Parts by weight Components must be mixed thoroughly
Mix ratio by volume — Part A:Part B 2:1 Parts by volume Volume measurement is not recommended for structural applications unless precautions ensure the correct ratio
Pot life 50 minutes 200 g mass at 77°F (25°C); ASTM D2471, water bath
Maximum recommended mixed quantity 450 g Do not mix larger quantities because hazardous heat buildup and uncontrolled decomposition may occur
Handling strength 24 hours At 77°F (25°C); full bond strength has not yet developed
Room-temperature cure 5–7 days At 77°F (25°C) to achieve normal performance
Example accelerated cure 1 hour at 180°F (82°C) — Complete cure; accelerated cures up to 200°F (93°C) are for small masses only
Shelf life — Part A and Part B 1 year Stored below 40°F (4°C)
Shelf life — Part A and Part B 6 months Stored below 77°F (25°C)
Shelf life — Part A and Part B 6 months Stored below 90°F (32°C)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers