LOCTITE EA E-05MR

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA E-05MR

Main features

  • Matched 1:1 Volume or Weight Mixing
  • Fast 10 to 15 Minute Fixture
  • Ultra-Clear Impact-Resistant Bonding

Product Description

LOCTITE EA E-05MR is a two-part, medium-viscosity epoxy adhesive that develops an ultra-clear, impact-resistant bondline through room-temperature cure. Resin and hardener mix 1:1 by volume or weight, with a 7 to 12 minute gel time at 22 deg C and a 10 to 15 minute fixture time on grit-blasted steel. The gap-filling adhesive is used on rough or poorly fitting surfaces and bonds supported materials including metals, ceramics, rigid plastics, and wood. Cured material combines high tensile strength with dielectric performance, making the clear system useful for general-purpose structural bonding where appearance and impact resistance matter.

Key features

  • Equal-Ratio Epoxy Mixing: Resin and hardener mix 1:1 by volume or weight.
  • Steel Fixture Time: Fixture time on grit-blasted steel is 10 to 15 minutes at 22 deg C under ISO 4587.
  • Impact-resistant clear bondline: Room-temperature cure forms an ultra-clear bondline with excellent impact resistance.

Applications

Applications include general-purpose bonding of supported metal, ceramic, rigid plastic, and wood substrates, including rough or poorly fitting surfaces.

Product Family

LOCTITE EA E-05MR

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Water white clear liquid
Chemistry TypeChemistry Type
Epoxy
Component SystemComponent System
Two Part (Resin | Hardener)
Specific GravitySpecific Gravity
1.16
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
39 °C
Mechanical Properties
ElongationElongation
4.5 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Component and mixed-material values are identified in the Method / condition column.

PropertyValueUnitMethod / condition
Viscosity18,000 to 25,000mPa sResin; cone and plate at 25 deg C and 100 s^-1
Viscosity18,000 to 25,000mPa sHardener; cone and plate at 25 deg C and 100 s^-1
Specific gravity1.16Mixed material at 25 deg C
Mix ratio1:1by volumeResin:hardener
Mix ratio1:1by weightResin:hardener
Gel time7 to 12minutesMixed material at 22 deg C
Fixture time10 to 15minutesISO 4587; grit-blasted steel; 22 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Glass transition temperature39deg CISO 11359-2; cured 5 days at 22 deg C
Hardness78Shore DISO 868; cured 5 days at 22 deg C
Dielectric breakdown strength34kV/mmIEC 60243-1; cured 5 days at 22 deg C
Tensile strength50N/mm^2ISO 527-3; cured 3 days at 22 deg C
Elongation4.5%ISO 527-3; cured 3 days at 22 deg C
Lap shear strength23N/mm^2ISO 4587; grit-blasted steel; 0.13 mm gap; cured 5 days at 22 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers