LOCTITE EA E-40FL

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE EA E-40FL

Main features

  • Flexible Dissimilar-Material Bonding
  • 40-Minute Working Window
  • Shock- and Impact-Resistant Bondline

Product Description

LOCTITE EA E-40FL is a two-part, toughened epoxy structural adhesive that cures to a flexible bondline and has a typical 40-minute working life. After a 1:1 volume mix, the adhesive cures at room temperature and is formulated for low-stress, high-impact bonding where flexibility is required. It bonds plastics, metals, glass, wood, ceramics, rubber, and masonry. The cured adhesive also provides electrical insulation and resistance to shock, impact, chemicals, and solvents. Larger mixed quantities and higher temperatures reduce the working time.

Key features

  • Flexible bondline: Typical elongation is 22% under ISO 527-2 for material cured at 25 deg C.
  • Assembly Working Life: Typical working life of the mixed adhesive is 40 minutes.
  • Shock and impact resistance: Toughened epoxy for low-stress bonding of dissimilar materials, including rubber hose to steel tubing.

Applications

Applications include bonding plastics, metals, glass, wood, ceramics, rubber, and masonry where a flexible bondline is required.

Product Family

LOCTITE EA E-40FL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Gray, opaque liquid
Chemistry TypeChemistry Type
Epoxy
Component SystemComponent System
Two Part (Resin | Hardener)
Pot LifePot Life
40 minutes
Specific GravitySpecific Gravity
1.2
Physical Properties
Tack-Free TimeTack-Free Time
130 minutes
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
30 °C
Mechanical Properties
ElongationElongation
22 %
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Resin, hardener, and mixed values are shown separately.

PropertyValueUnitMethod / condition
Mix ratio, resin : hardener1 : 1By volume
Mix ratio, resin : hardener100 : 85By weight
Resin viscosity60,000 to 90,000mPa sLMS range; Brookfield RVT; 25 deg C; spindle 7; 10 rpm
Hardener viscosity50,000 to 85,000mPa sLMS range; Brookfield RVT; 25 deg C; spindle 7; 10 rpm
Working life40minTypical; mixed material
Tack-free time130minTypical; mixed material
Technical properties

Cured / final-state properties

PropertyValueUnitMethod / condition
Glass transition temperature, Tg30deg CTypical; cured at 25 deg C
Shore hardness75Shore DTypical; ISO 868; cured at 25 deg C
Elongation22%Typical; ISO 527-2; cured at 25 deg C
Tensile strength16N/mm^2Typical; ISO 527-2; cured at 25 deg C
Dielectric breakdown strength16kV/mmTypical; IEC 60243-1; cured at 25 deg C
Lap shear strength, aluminum25.9N/mm^2Typical; acid etched and abraded; 0.1 to 0.2 mm gap; cured 3 days at 22 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers