LOCTITE EDAG PF 410 E&C
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

Main features
- Screen printable
- Excellent print definition
- Silver filled
Product Description
LOCTITE EDAG PF 410 E&C is designed for production of flexible circuitry. This material can be used on a variety of substrates and is applicable with manual, semi automatic or high speed reel to reel screen printing equipment.
LOCTITE EDAG PF 410 E&C is passed over a triple roll mill to remove small particles. It offers extended screen residence time and excellent print definition with superior adhesion to polyester film.
Drying Cycle
- 30 minutes @ 80°C or
- 15 minutes @ 120°C
LOCTITE EDAG PF 410 E&C can be dried immediately after printing at temperatures between 80 to 140°C
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Additional Information
Optimal Storage : 5 to 30 °C
TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
-Applied dry coating thickness , μm 8 to 12
Emulsion Thickness
-Emulsion Thickness , μm 20 to 40
Recommended Squeegee
-Polyurethane , durometer 70 to 75
Recommended Screen Type
-Monofilament polyester screen, threads/cm 68 to 110
-Stainless steel screen , threads/cm 90 to 154
Printing Equipment Type
-Manual
-Semi-automatic
-High speed reel-to-reel