LOCTITE M2013RS

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

LOCTITE M2013RS

Main features

  • One-Component Screen Printing
  • 2-Minute 200 deg C Drying
  • 1% Laser-Trimming Linearity

Product Description

LOCTITE M2013RS is a one-component conductive ink supplied in a 1 kg container for screen-printing printed-electronics features. Compatible substrates include FR-3, FR-4, CEM-1, CEM-3, polyester sulfone, and ceramic. Its optimum drying cycle is 2 minutes at 200 deg C, followed by heat or infrared cure. It is laser trimmable with 1% linearity and has high wear resistance. The one-component format combines screen-printing application with a defined thermal drying and cure sequence for conductive printed features.

Key features

  • Screen-Printable One-Component Ink: The format supports screen printing of conductive printed-electronics features.
  • Thermal Drying Cycle: Optimum drying is 2 minutes at 200 deg C.
  • Laser-Trim Control: Laser-trimming linearity is 1%.

Applications

Compatible substrates include FR-3, FR-4, CEM-1, CEM-3, polyester sulfone, and ceramic.

Product Family

LOCTITE M2013RS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Black
Thermal Properties
Flash PointFlash Point
95 °C
Physical Properties
VOCVOC
45 - 55 %

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers