LOCTITE N-5000

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

LOCTITE N-5000

Main features

  • -29 to 1315 deg C Range
  • Low-Contaminant Nickel-Graphite Formula
  • 0.18 Stainless-Fastener Torque Coefficient

Product Description

LOCTITE LB N-5000 is a one-component nickel-and-graphite anti-seize formulation in a petroleum carrier for high-purity threaded-fastener and metal-fit service. The formulation contains low practical levels of halogens, sulfur, heavy metals, and copper. Its typical operating range is -29 to 1315 deg C. Typical as-supplied data include specific gravity 1.12 to 1.27 at 25 deg C and unworked penetration of 330 to 380 1/10 mm by ISO 2137. On the specified 12.7 mm 304 stainless-steel fastener configuration, the torque coefficient is 0.18.

Key features

  • High-Temperature Application: Typical operating range is -29 to 1315 deg C.
  • High-Purity Nickel-Graphite Blend: Nickel and graphite flake in a petroleum carrier with low practical levels of halogens, sulfur, heavy metals, and copper.
  • 0.18 Stainless-Fastener Torque Coefficient: Measured on 12.7 mm 304 stainless-steel grade 8 bolts with grade 5 nuts.

Applications

Threaded metal fasteners, bolts, studs, valves, pipe fittings, slip fits, and press fits where high-purity anti-seize is specified.

Product Family

LOCTITE N-5000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Silver colored paste
Chemistry TypeChemistry Type
Nickel-based
Specific GravitySpecific Gravity
1.12 to 1.27
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Specific gravity1.12 to 1.27Typical; 25 deg C
Unworked penetration330 to 3801/10 mmTypical; ISO 2137
Chloride50ppmMaximum
Sulfur100ppmMaximum
Copper50ppmMaximum
Cadmium2ppmMaximum

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers