LOCTITE PC 3965

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE PC3965

Main features

  • Equal-Ratio Epoxy Mixing
  • 3 to 4 Minute Working Life
  • 23.9 N/mm^2 Steel Lap Shear

Product Description

LOCTITE PC 3965 is a two-part steel-filled epoxy repair adhesive supplied as a 50 mL dual-cartridge system with resin and hardener. The mix ratio is 1:1 by volume or 100:73 by weight, with a 3 to 4 minute working life and 4 to 6 minute gel time at 25 deg C. It is a non-sag paste for overhead and vertical repairs and hardens in 10 minutes. After cure, it can be machined, drilled, tapped, or filed. Supported substrates include steel, cast iron, stainless steel, concrete, copper, aluminum, and clean abraded bronze.

Key features

  • Equal-Ratio Volume Mixing: Resin and hardener mix 1:1 by volume; the weight ratio is 100:73.
  • 3 to 4 Minute Working Life: Working life is 3 to 4 minutes at 25 deg C; gel time is 4 to 6 minutes.
  • 23.9 N/mm^2 Steel Lap Shear: Typical lap shear strength is 23.9 N/mm^2 by ISO 4587 on grit-blasted mild steel.

Applications

Repair and bonding of steel, cast iron, stainless steel, concrete, copper, aluminum, and clean abraded bronze.

Product Family

LOCTITE PC 3965

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Metallic gray
Chemistry TypeChemistry Type
Epoxy
Component SystemComponent System
Two Part (Resin | Hardener)
Pot LifePot Life
3 to 4 minutes
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
58 °C
Mechanical Properties
ElongationElongation
0.64 %
Electrical Properties
Volume ResistivityVolume Resistivity
0.47×10¹⁵ Ohms⋅cm
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Mix ratio by volume1:1Resin : hardener
Mix ratio by weight100:73Resin : hardener
Resin viscosity95,000 to 115,000mPa sTypical; Brookfield RV, 25 deg C, spindle 7, 20 rpm
Hardener viscosity130,000 to 160,000mPa sTypical; Brookfield RV, 25 deg C, spindle 2, 20 rpm
Working life3 to 4minutes25 deg C
Gel time4 to 6minutes25 deg C
Technical properties

Cured material

Cured at 25 deg C except where noted.

PropertyValueUnitMethod / condition
Tensile strength20N/mm^2Typical; ISO 527-2
Compressive strength68N/mm^2Typical; ISO 604
Flexural strength52N/mm^2Typical; ASTM D790
Shore hardness62Shore DTypical; ISO 868
Elongation0.64%Typical; ISO 527-2
Thermal conductivity0.286W/(m K)Typical; ASTM F433
Lap shear strength23.9N/mm^2Typical; ISO 4587; grit-blasted mild steel

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers