LOCTITE PC 6249

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE PC6249

Main features

  • No-Mix Epoxy Application
  • Multi-Method Floor Coating
  • At Least 0.8 Wet Friction

Product Description

LOCTITE PC 6249 is a one-component epoxy non-slip floor and deck coating for concrete and steel areas with heavy pedestrian or light rolling traffic. Typical uncured volume solids is 62%. Application methods include roller, spray, or trowel. At 21 deg C, light pedestrian dry time is 12 hours and heavy pedestrian dry time is 72 hours, while tack-free time is up to 6 hours. After cure at 21 deg C, typical ASTM F609 coefficient of friction is at least 1.0 dry and at least 0.8 wet. The coating is used on ramps, walkways, loading docks, and similar floor or deck surfaces where a non-slip finish is required.

Key features

  • 62% Typical Volume Solids: Typical uncured volume solids is 62%.
  • Roller, Spray, or Trowel Application: Application methods include roller, spray, and trowel.
  • ASTM F609 Friction: After cure at 21 deg C, typical coefficient of friction is at least 1.0 dry and at least 0.8 wet.

Applications

Ramps, walkways, loading docks, and similar concrete or steel floor and deck surfaces.

Product Family

LOCTITE PC 6249

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Black, Grey
SolidsSolids
62 %
Physical Properties
Tack-Free TimeTack-Free Time
≤360 minutes
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Volume solids62%Typical; uncured material
Coverage4.6m^2 per 3.78 LTypical; roller application
Coverage5.6m^2 per 3.78 LTypical; spray application
Coverage3.7m^2 per 3.78 LTypical; trowel application
Sag resistance2mmTypical; no sagging; uncured material
Technical properties

Cured coating

PropertyValueUnitMethod / condition
Coefficient of friction - dryAt least 1.0Typical; ASTM F609; cured at 21 deg C
Coefficient of friction - wetAt least 0.8Typical; ASTM F609; cured at 21 deg C
Impact resistance50cm*kgTypical; cured at 21 deg C
FlexibilityUp to 100mmTypical; cured at 21 deg C
Water resistanceNo swelling, foaming, or flakingTypical; 15 days; cured at 21 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers