LOCTITE PC 6311

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE PC6311

Main features

  • Heavy-Vehicular Non-Slip Coating
  • 8.9:1 Volume Mix Ratio
  • 1.05 Dry and Wet Friction

Product Description

LOCTITE PC 6311 is a two-component epoxy non-slip coating for industrial floors and decks exposed to heavy vehicular traffic. Resin and hardener mix at 17.6:1 by weight or 8.9:1 by volume and cure at room temperature. Typical uncured volume solids is 70%. Application methods include roller, spray, or trowel. At 21 deg C, light pedestrian dry time is 12 hours and heavy pedestrian dry time is 48 hours. After cure at 21 deg C, typical ASTM F609 coefficient of friction is 1.05 in both dry and wet tests. Typical dry service temperature is -30 to 60 deg C.

Key features

  • 8.9:1 Volume Mixing: The resin-to-hardener ratio is 8.9:1 by volume and 17.6:1 by weight.
  • Typical 70% Volume Solids: Typical uncured volume solids is 70%.
  • 1.05 Dry and Wet Friction: Typical ASTM F609 coefficient of friction is 1.05 in both dry and wet tests after cure at 21 deg C.

Applications

Industrial floor and deck areas exposed to heavy vehicular traffic, including concrete or steel ramps, walkways, and loading docks.

Product Family

LOCTITE PC 6311

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two Part (Resin | Hardener)
SolidsSolids
70 %
Physical Properties
VOCVOC
250 g/L
Other Properties
Storage TemperatureStorage Temperature
8 °C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Mix ratio8.9:1Resin:hardener by volume
Mix ratio17.6:1Resin:hardener by weight
Volume solids70%Typical; uncured material
VOC250g/LTypical; uncured material
Coverage3.7m^2 per 3.78 LTypical; roller application
Coverage5.6m^2 per 3.78 LTypical; spray application
Coverage4.6m^2 per 3.78 LTypical; trowel application
Technical properties

Cured coating

PropertyValueUnitMethod / condition
Coefficient of friction - dry1.05Typical; ASTM F609; cured at 21 deg C
Coefficient of friction - wet1.05Typical; ASTM F609; cured at 21 deg C
Dry service temperature-30 to 60deg CTypical; heavy vehicular traffic application

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers