LOCTITE PC 7202

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE PC7202

Main features

  • Self-Leveling Machinery Chocking
  • 10 to 15-Minute Working Window
  • 110 N/mm^2 Cured Compressive Strength

Product Description

LOCTITE PC 7202 is a two-component epoxy chocking system for installing main engines, drive engines, winches, hoists, and other deck-mounted equipment. Resin and hardener mix at 100:11.6 by volume or 100:6.9 by weight. Typical data at 25 deg C include mixed density of 1.5 g/cm^3, working time of 10 to 15 minutes, and cure time of 24 hours. After 24 hours at 25 deg C, typical cured properties include Shore D 90 hardness, 38 N/mm^2 tensile strength, and 110 N/mm^2 compressive strength. The 100% solids epoxy is self-leveling for machinery chocking and grouting applications.

Key features

  • 100:11.6 Volume Mixing: The resin-to-hardener mix ratio is 100:11.6 by volume and 100:6.9 by weight.
  • 10 to 15-Minute Working Time: Typical working time is 10 to 15 minutes at 25 deg C; typical cure time is 24 hours at 25 deg C.
  • 110 N/mm^2 Compressive Strength: After 24 hours at 25 deg C, typical compressive strength is 110 N/mm^2 by ISO 604.

Applications

Chocking and grouting of main engines, drive engines, winches, hoists, and deck-mounted equipment.

Product Family

LOCTITE PC 7202

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Orange or green liquid
Component SystemComponent System
Two Part (Resin | Hardener)
Density (g)Density (g)
1.5 g/cm3
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
110 °C
Other Properties
Storage TemperatureStorage Temperature
8°C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Mix ratio100:11.6Resin:hardener by volume
Mix ratio100:6.9Resin:hardener by weight
Orange resin viscosity80,000 to 110,000mPa sTypical; Brookfield RVDV3; spindle 7; 20 rpm; 25 deg C
Green resin viscosity85,000 to 105,000mPa sTypical; Brookfield RVDV3; spindle 7; 20 rpm; 25 deg C
Hardener viscosity32.6mPa sTypical; cone and plate; shear rate 3,000 s^-1; 25 deg C
Mixed density1.5g/cm^3Typical; ISO 1675; 25 deg C
Technical properties

Cured material

PropertyValueUnitMethod / condition
Shore hardness90Shore DTypical; ISO 868; cured 24 hours at 25 deg C
Tensile strength38N/mm^2Typical; ISO 527-2; cured 24 hours at 25 deg C
Compressive strength110N/mm^2Typical; ISO 604; cured 24 hours at 25 deg C
Compressive modulus2,760N/mm^2Typical; ISO 604; cured 24 hours at 25 deg C
Tensile modulus8,400N/mm^2Typical; ASTM D638; cured 24 hours at 25 deg C
Glass transition temperature110deg CTypical; TMA; ISO 11359-2; cured 24 hours at 25 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers