LOCTITE PC 7210

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE PC7210

Main features

  • 30-Minute 25 deg C Working Life
  • 35 N/mm^2 Steel Lap Shear
  • Composite Pipe and Tank Repair

Product Description

LOCTITE PC 7210 is a two-component toughened epoxy repair paste for pipe, tank, and structural repair, including composite repair systems used with LOCTITE PC 5085 fabric. Resin and hardener mix at 100:55 by volume or 100:40 by weight and cure at room temperature after mixing. Typical data at 25 deg C include resin viscosity of 14,000 mPa s, hardener viscosity of 11,500 mPa s, and mixed specific gravity of 1.2. Typical working life is 30 minutes at 25 deg C and 20 minutes at 40 deg C. After seven days at 22 deg C, typical cured LOCTITE PC 7210 data include Shore D 77 hardness, a 100 deg C glass transition temperature, and 35 N/mm^2 lap shear strength on grit-blasted mild steel by ISO 4587.

Key features

  • 100:55 Volume Mixing: The resin-to-hardener ratio is 100:55 by volume and 100:40 by weight.
  • Temperature-Dependent Working Life: Typical working life is 30 minutes at 25 deg C and 20 minutes at 40 deg C.
  • 35 N/mm^2 Steel Lap Shear: After seven days at 22 deg C, typical lap shear strength is 35 N/mm^2 on grit-blasted mild steel by ISO 4587.

Applications

Pipe, tank, and structural repair, including composite repair systems used with LOCTITE PC 5085 fabric.

Product Family

LOCTITE PC 7210

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component SystemComponent System
Two Part (Resin | Hardener)
Specific GravitySpecific Gravity
1.2
Work life @25°CWork life @25°C
0.5 hours
Mechanical Properties
ElongationElongation
2.0 %
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
100 °C
Other Properties
Storage TemperatureStorage Temperature
8°C to 21 °C

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
Mix ratio100:55Resin:hardener by volume
Mix ratio100:40Resin:hardener by weight
Resin specific gravity1.32Typical; 25 deg C
Resin viscosity14,000mPa sTypical; cone and plate; 25 deg C
Hardener specific gravity0.97Typical; 25 deg C
Hardener viscosity11,500mPa sTypical; cone and plate; 25 deg C
Mixed specific gravity1.2Typical; 25 deg C
Vertical sag resistance1.3mmTypical; ASTM D4400; mixed material at 25 deg C and 40 deg C
Technical properties

Cured adhesive

PropertyValueUnitMethod / condition
Glass transition temperature100deg CTypical; DMA; ASTM E1640; cured 7 days at 22 deg C
Shore hardness77Shore DTypical; ISO 868; cured 7 days at 22 deg C
Lap shear strength - mild steel35N/mm^2Typical; ISO 4587; grit blasted; cured 7 days at 22 deg C
Lap shear strength - aluminum29N/mm^2Typical; ISO 4587; grit blasted; cured 7 days at 22 deg C
Lap shear strength - stainless steel27N/mm^2Typical; ISO 4587; grit blasted; cured 7 days at 22 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers