LOCTITE PE3164
Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

Main features
- 105 cP Hardener Viscosity
- 2:1 PE 3140 Volume Mixing
- 10 to 15 Minute System Work Time
Product Description
LOCTITE PE 3164 is the clear epoxy hardener component used as Part B with LOCTITE PE 3140 resin in a two-part potting system. As supplied, PE 3164 has 105 cP viscosity at 25 deg C using spindle 2 at 20 rpm and a specific gravity of 0.97. The PE 3140 and PE 3164 system mixes at 2:1 resin-to-hardener by volume and has a 10 to 15 minute work time for a 400 g mass at 25 deg C. Cure time is 16 hours at 25 deg C or 2 hours at 66 deg C.
Key features
- 105 cP Hardener Viscosity: PE 3164 hardener viscosity is 105 cP at 25 deg C using spindle 2 at 20 rpm.
- 2:1 PE 3140 Volume Mixing: The PE 3140 and PE 3164 system uses a 2:1 resin-to-hardener ratio by volume.
- Paired-System Working Time: The PE 3140 and PE 3164 system has a 10 to 15 minute work time for a 400 g mass at 25 deg C.
Applications
Hardener component for the LOCTITE PE 3140 two-part potting system.
Technical Specifications
General Properties
Physical Properties
Additional Information
As supplied
Values apply to the LOCTITE PE 3164 hardener component only.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Clear | PE 3164 hardener, as supplied | |
| Viscosity | 105 | cP | PE 3164 hardener; spindle 2, 20 rpm, 25 deg C |
| Specific gravity | 0.97 | PE 3164 hardener, as supplied | |
| Storage temperature | 8 to 28 | deg C | Unopened container unless otherwise labeled |