LORD 307-2

Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations

LORD 307-2

Main features

  • 20,000 to 57,000 cP Hardener Viscosity
  • 1:1 General-Purpose Volume Mix
  • 1- to 2-Hour System Working Time

Product Description

LORD 307-2 is the Part B hardener used with LORD 305-1 resin in a two-component, medium-viscosity epoxy adhesive system. As supplied, the hardener is a clear amber liquid with a typical viscosity of 20,000 to 57,000 cP at 25 deg C and density of 947 to 995 kg/m^3. For general-purpose mixed-stress joints, LORD 305-1/307-2 uses a 1:1 resin-to-hardener volume ratio. A 54 g mixed mass has a typical working time of 1 to 2 hours at 24 deg C, with handling strength in 8 to 16 hours and full strength in 24 to 48 hours at 18 deg C or higher.

Key features

  • Hardener Rheology: Typical LORD 307-2 viscosity is 20,000 to 57,000 cP at 25 deg C using Brookfield HBF, spindle 2 at 10 rpm.
  • System Mixing: The LORD 305-1/307-2 general-purpose configuration uses a 1:1 resin-to-hardener ratio by volume.
  • Mixed-System Work Time: A 54 g LORD 305-1/307-2 mixed mass has a typical working time of 1 to 2 hours at 24 deg C.

Applications

When combined with LORD 305-1, system uses include assembling food-processing machinery such as gaskets, bushings, shock-absorbing devices, and rubber rolls, plus bonding prepared metals and prepared rubber.

Product Family

LORD 307-2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Clear Amber Liqui
DensityDensity
947- 995 kg/m3
Mix RatioMix Ratio
1:1
SolidsSolids
100 %
Physical Properties
ViscosityViscosity
20,000 - 57,000 mPa.s
Young's modulusYoung's modulus
748 MPa
Mechanical Properties
ElongationElongation
31 %
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
61 °C

Additional Information

Technical properties

As-supplied / before-processing properties

LORD 307-2 component-specific values; mixed and cured properties apply to the LORD 305-1/307-2 system.

PropertyValueUnitMethod / condition
AppearanceClear amber liquidTypical as supplied
Viscosity20,000 to 57,000cPTypical at 25 deg C; Brookfield HBF; spindle 2; 10 rpm
Density947 to 995kg/m^3Typical as supplied

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers