LORD 312-A

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD 312-A

Main features

  • 1.13 g/cm^3 Resin Density
  • 0.00% Volatile Content by Weight
  • Potting and Thin-Film Encapsulation

Product Description

LORD 312-A is the Part A resin component of the low-viscosity LORD 312-A/312-B two-part epoxy system used for potting and thin-film encapsulation. As supplied, the component is a yellow liquid with a typical density of 1.13 g/cm^3 and 0.00% volatile content by weight. It is combined with LORD 312-B before application, forming the mixed epoxy used for potting and thin-film encapsulation. Cured properties apply to the complete LORD 312-A/312-B system rather than to Part A alone.

Key features

  • Resin Identification: Yellow liquid Part A has a typical as-supplied density of 1.13 g/cm^3.
  • As-Supplied Volatiles: Typical volatile content by weight is 0.00%.
  • System Application: When paired with LORD 312-B, the mixed epoxy is used for potting and thin-film encapsulation.
Product Family

LORD 312-A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

Physical Properties
Viscosity (Part B)Viscosity (Part B)
750-2500 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers