LORD 7545-A

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LORD 7545-A

Main features

  • Multi-Curative Work-Time Flexibility
  • Equal-Volume System Mixing
  • Manual or Automated Dispensing

Product Description

LORD 7545-A Resin is the brown paste resin component used with compatible LORD 7545 curatives to form equal-mix, two-component urethane adhesive systems. It has a typical Brookfield viscosity of 25,000 to 70,000 cP at 77 deg F (25 deg C) and a density of 12.5 to 12.8 lb/gal. The resin mixes 1:1 by volume with the selected curative, allowing the 7545 system to be configured for working times from 1.5 to 65 minutes at 75 deg F (24 deg C). Handheld cartridges or automatic meter/mix/dispense equipment can be used for application. LORD 7545-A is supplied as Part 1 and is not a complete adhesive without an appropriate curative.

Key features

  • Common resin component: Pairs with compatible LORD 7545 curatives to create configuration-specific working and handling times.
  • Equal-volume mixing: Mixes with the selected curative at a 1:1 ratio by volume for cartridge or bulk dispensing.
  • Flexible dispensing methods: Can be applied with handheld cartridges or automatic meter/mix/dispense equipment as part of the mixed system.
Product Family

LORD 7545-A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Brown/Black/Off-White
Density (g)Density (g)
10.6-12.8 g/cm3
Mix RatioMix Ratio
1:1
SolidsSolids
100 %
Physical Properties
ViscosityViscosity
230000-650000 mPa.s
Thermal Properties
Flash PointFlash Point
93 °C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
47 °C
Mechanical Properties
ElongationElongation
72 %
Chemical Properties
Moisture absorptionMoisture absorption
1 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values apply to the standalone LORD 7545-A resin component.

PropertyValueUnitMethod / condition
AppearanceBrown paste-LORD 7545-A resin
Viscosity25,000 to 70,000cPTypical; Brookfield at 77 deg F (25 deg C); LORD 7545-A resin
Density12.5 to 12.8lb/galTypical; LORD 7545-A resin (1498 to 1534 kg/m^3)
Flash point>200deg FTypical; closed cup; LORD 7545-A resin (>93 deg C)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers