LORD 7545F

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

LORD 7545F

Main features

  • 45 to 65 Minute A/F Work Time
  • Manual or Automated A/F Dispensing
  • Non-Sag A/F Vertical Placement

Product Description

LORD 7545-F Curative is a curative component that extends the processing window of LORD 7545-A/F equal-mix urethane adhesive systems. The off-white paste has a typical Brookfield viscosity of 230,000 to 650,000 cP at 77 deg F (25 deg C) and mixes with LORD 7545-A resin at 1:1 by volume or 1:0.85 by weight. This A/F configuration provides 45 to 65 minutes of typical working time and reaches handling strength in 4 to 5 hours at 75 deg F (24 deg C), supporting assemblies that need more placement time. The system can be dispensed with handheld cartridges or automatic equipment and retains non-sag behavior on vertical or overhead surfaces. LORD 7545-F is a curative component, not a standalone adhesive.

Key features

  • Extended A/F working window: Provides 45 to 65 minutes of typical working time at 75 deg F (24 deg C) when mixed with LORD 7545-A.
  • Flexible dispensing methods: Supports handheld cartridge or automatic meter/mix/dispense application as part of the A/F system.
  • Non-sag system placement: The mixed 7545 system retains position on vertical or overhead surfaces.
Product Family

LORD 7545F

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Brown/Black/Off-White
Density (g)Density (g)
10.6-12.8 g/cm3
Mix RatioMix Ratio
1:1
SolidsSolids
100 %
Physical Properties
ViscosityViscosity
230000-650000 mPa.s
Thermal Properties
Flash PointFlash Point
93 °C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
47 °C
Mechanical Properties
ElongationElongation
72 %
Chemical Properties
Moisture absorptionMoisture absorption
1 %

Additional Information

Technical properties

As-supplied / before-processing properties

Values apply to the standalone LORD 7545-F curative component.

PropertyValueUnitMethod / condition
AppearanceOff-white paste-LORD 7545-F curative
Viscosity230,000 to 650,000cPTypical; Brookfield at 77 deg F (25 deg C); LORD 7545-F curative
Density10.5 to 11.1lb/galTypical; LORD 7545-F curative (1258 to 1330 kg/m^3)
Flash point>200deg FTypical; closed cup; LORD 7545-F curative (>93 deg C)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers